C51000 Phosphor Bronze (5% Sn)
UNS C51000 | ASTM B103 / B139 / B159 | AMS4510 / AMS4625
C51000 is a wrought tin–phosphorus bronze strengthened by cold work. Its nearest European grade is CW451K (CuSn5, old BS PB102), but the UNS and EN chemistry limits differ.
It is not PB1, which is a cast 10–11% tin phosphor bronze.
Imagery is illustrative metal product forms, not certified C51000 stock or evidence of Quest stockholding.
Raw & semi-finished materials
Available material forms
ASTM B103 flat products, B139 rod/bar/shapes, B159 wire. Confirm forms, sizes and availability at enquiry.
- Strip, sheet and plate
- Rod and bar
- Wire
Material overview
C51000 Phosphor Bronze (5% Sn)
A wrought 5% tin phosphor bronze with good spring properties and cold formability, supplied in strip, rod and wire.
- Flat and wire properties are separate conditions; wire is much stronger at the same temper.
- CW451K: Sn 4.5–5.5%, P 0.01–0.4% (CDA UK) versus C51000 Sn 4.2–5.8%, P 0.03–0.35%.
Designations and specifications
| Designation / standard | Scope and qualification |
|---|---|
| UNS | C51000 |
| EN / BS | Approximately CW451K CuSn5 / PB102 — chemistry limits differ |
| ASTM B103 / B139 / B159 | Flat products / rod, bar and shapes / wire |
| AMS4510 | Spring-temper sheet, strip and plate |
| AMS4625 | Hard-temper bars, rods and tubing |
| EN 1652 / EN 12163 | Flat products / rod for CW451K |
Specification review
Technical verification requirements
Mechanical
O60/H02 flat section not stated; specification minima not shown.
Obtain ordered-specification tables.
Grade selection
Phosphor and silicon bronzes — distinct grades
| Grade | Type | Key chemistry (limits) | Conductivity (CDA, 20°C) | Nearest EN / BS |
|---|---|---|---|---|
| C51000 | Wrought phosphor bronze | Sn 4.2–5.8%; P 0.03–0.35% | 15% IACS (5% Sn, 0.2% P basis) | Approx. CW451K CuSn5 / PB102 |
| C52100 | Wrought phosphor bronze | Sn 7.0–9.0%; P 0.03–0.35% | 13% IACS | Approx. CW453K CuSn8 / PB104 |
| PB1 | Cast phosphor bronze | Sn 10.0–11.5%; P 0.5–1.0% (EN 1982 CC481K casting) | Not stated as % IACS | Cross-referenced to CC481K CuSn11P-C |
| C65100 | Wrought low-silicon bronze | Si 0.8–2.0% | 12% IACS | Not CW116C |
| C65500 | Wrought high-silicon bronze | Si 2.8–3.8%; Mn 0.50–1.3% | 7% IACS | Related to CW116C CuSi3Mn1 / CS101 |
PB1 is a cast alloy and is not CW451K. UNS and EN chemistries differ, so “approximately” equivalent grades are not automatically cross-certified. Properties are never transferred between these grades.
Engineering reference
Technical data
| Element | Mass % |
|---|---|
| Tin | 4.2–5.8 |
| Phosphorus | 0.03–0.35 |
| Lead | 0.05 max |
| Zinc | 0.30 max |
| Iron | 0.10 max |
| Copper | Remainder |
| Cu + named elements | 99.5 min |
Copper Development Association — C51000 alloy record
| Property | Value | Basis |
|---|---|---|
| Density | 8.86 g/cm³ | From CDA specific gravity |
| Electrical conductivity | 15% IACS | 20°C; alloy with 5% Sn, 0.2% P |
| Thermal conductivity | 69.2 W/(m·K) | 20°C |
| Mean CTE 20–300°C | 17.8 × 10⁻⁶/K | Temper not stated |
| Elastic modulus (tension) | 110 GPa | Temperature not stated |
CDA generic values; temper, form and section not stated. Conductivity depends on composition.
Copper Development Association — C51000 alloy record
Flat — O60 soft annealed
| Section | Tensile strength | Yield (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| Section not stated | 50 ksi (345 MPa) | Not reported | 40% | Not reported |
CDA typical values at 20°C, not specification minima.
Copper Development Association — C51000 alloy record
Flat — H02 half hard
| Section | Tensile strength | Yield (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| Section not stated | 66 ksi (455 MPa) | 54 ksi (372 MPa) | 24% | Not reported |
CDA typical values at 20°C, not specification minima.
Copper Development Association — C51000 alloy record
Flat — H04 hard
| Section | Tensile strength | Yield (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| 0.04 in (1.0 mm) | 84 ksi (579 MPa) | 80 ksi (552 MPa) | 7% | Not reported |
CDA typical values at 20°C, not specification minima.
Copper Development Association — C51000 alloy record
Flat — H08 spring
| Section | Tensile strength | Yield (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| 0.04 in (1.0 mm) | 103 ksi (710 MPa) | 99 ksi (683 MPa) | 3% | Not reported |
CDA typical values at 20°C, not specification minima.
Copper Development Association — C51000 alloy record
Wire — H02 / H04 / H08
| Section | Tensile strength | Yield (0.2% offset) | Elongation | Hardness |
|---|---|---|---|---|
| H02, 0.08 in (2.0 mm) | 85 ksi (586 MPa) | Not reported | 8% | Not reported |
| H04, 0.08 in | 110 ksi (758 MPa) | Not reported | 3% | Not reported |
| H08, 0.08 in | 140 ksi (965 MPa) | Not reported | 2% | Not reported |
CDA typical values at 20°C, not specification minima.
Copper Development Association — C51000 alloy record
Annealing range (CDA)
482–677°C (900–1250°F). Section, hold time and atmosphere are not stated; not a complete production schedule.
Temper designations
O60 soft anneal; H02 half hard; H04 hard; H08 spring. Grain-size anneals (OS) and O61 are separate tempers and are not relabelled.
Agree temper with the product specification.
Copper Development Association — C51000 alloy record
Typical applications
Engineering applications
- Springs, contacts and connectors
- Bellows and diaphragms
- Bearing plates and wear components
- Fasteners
Subsequent manufacturing
Machining & processing
Cold working
Excellent cold workability (CDA); hot forming poor.
Not heat-treatable
Strength comes from cold work (H tempers); annealing softens. Temper must be specified with the product form.
Application evidence
Listed applications are source-cited categories, not claims of stock or component approval.
Material certification & testing
Documentation must be agreed for the actual UNS/EN grade, product or casting specification, form, temper and section.
No certificate, approval or grade equivalence is automatic. “Nearest” or “related” designations do not certify compliance; quotation controls remain disabled.
- EN 10204 3.1 material certificate, where agreed with the supplier
- Certificate of Conformity
- Cast / lot traceability to the producing mill or foundry
- Chemical analysis and mechanical test results to the ordered specification
- Ultrasonic, impact or corrosion-related testing only where the ordered specification requires it