Materials Supply / Copper & Copper-Base Alloys
C10200 Oxygen-Free Copper (OF)
OF | UNS C10200 | Cu-OF CW008A
C10200 is oxygen-free copper. Like OFE it resists the oxide-related hydrogen embrittlement that affects ETP copper, but its designation does not limit individual impurities.
It is not interchangeable with C10100 (OFE) where electron-device purity is specified.
Imagery is illustrative metal product forms, not certified C10200 stock or evidence of Quest stockholding.
Raw & semi-finished materials
Available material forms
CDA lists flat products, rod/bar/shapes, tube and wire. Confirm forms, sizes and availability at enquiry.
- Sheet, strip and plate
- Rod, bar and bus bar
- Tube
- Wire
Material overview
C10200 Oxygen-Free Copper (OF)
Oxygen-free copper with ≥99.95% Cu+Ag and ≤10 ppm oxygen, for conductors and components brazed or used in reducing atmospheres.
- Annealed minimum conductivity is 100% IACS at 20°C; CDA tables 101% IACS as a property value — the minimum governs.
- Aurubis Cu-OF additionally limits Bi and Pb; these are producer requirements.
Designations and specifications
| Designation / standard | Scope and qualification |
|---|---|
| UNS / EN | C10200; Cu-OF, CW008A |
| ASTM B170 Grade 2 | Refinery shapes |
| ASTM B152 / B187 / B49 | Flat products / bus bar, rod and shapes / redraw rod (CDA) |
| AMS 4501 | Listed by CDA for light-cold-rolled flat products; current revision not verified |
| EN 13601 / EN 1652 / EN 12163 | Product families only; grade inclusion not verified |
Copper Development Association — C10200 alloy record
Specification review
Technical verification requirements
Chemistry
No individual impurity limits in CDA designation; Aurubis 99.99/99.95% wording conflict.
Specify impurity limits and use mill certificate.
Grade selection
C10100, C10200 and C11000 — distinct coppers
| Aspect | C10100 (OFE) | C10200 (OF) | C11000 (ETP) |
|---|---|---|---|
| Type | Oxygen-free electronic | Oxygen-free | Electrolytic tough pitch (contains oxygen) |
| Copper (CDA designation) | ≥99.99% excl. Ag | ≥99.95% incl. Ag | ≥99.90% incl. Ag |
| Oxygen (CDA designation) | ≤5 ppm | ≤10 ppm | No limit in CDA designation; Aurubis strip ≤400 ppm |
| Individual impurity limits | 16 elements limited | None in CDA designation | None in CDA designation |
| Min. conductivity, annealed, 20°C | 101% IACS | 100% IACS | 100% IACS |
| Hydrogen embrittlement in reducing atmospheres | Resistant to oxide-related mechanism | Resistant to oxide-related mechanism | Susceptible |
Designation limits are not product-specification acceptance requirements. ETP must not be substituted for OF/OFE where hydrogen brazing, vacuum or reducing-atmosphere service applies.
Copper Development Association — C10100 alloy record
Engineering reference
Technical data
| Element | CDA designation | Aurubis Cu-OF |
|---|---|---|
| Copper + silver | 99.95% min | 99.95% min |
| Oxygen | 10 ppm max | 10 ppm max |
| Bismuth | Not limited | 5 ppm max |
| Lead | Not limited | 50 ppm max |
OFE impurity limits are not applied to OF. Aurubis narrative states 99.99% Cu while its table states 99.95% — the table and certificate govern.
| Property | Value | Basis |
|---|---|---|
| Electrical conductivity | 100% IACS | Annealed, 20°C — minimum |
| Thermal conductivity | ≈391 W/(m·K) (226 Btu/h·ft·°F) | 20°C; temper not stated |
| Density | 8.94 g/cm³ (0.323 lb/in³) | 20°C |
| Mean CTE 20–100°C | 16.9 × 10⁻⁶/K (9.4 × 10⁻⁶/°F) | Temper not stated |
| Mean CTE 20–200°C | 17.3 × 10⁻⁶/K (9.6 × 10⁻⁶/°F) | Temper not stated |
| Mean CTE 20–300°C | 17.6 × 10⁻⁶/K (9.8 × 10⁻⁶/°F) | Temper not stated |
| Elastic modulus (tension) | ≈117 GPa (17,000 ksi) | Temperature and temper not stated |
| Melting range | 1083°C | CDA |
CDA values; metric figures converted from customary units. Cold work reduces conductivity slightly; confirm for the ordered temper. Aurubis strip datasheets report 127 GPa modulus — kept separate.
Copper Development Association — C10200 alloy record
OS050 annealed (0.050 mm grain) — flat, CDA typical
| Property | CDA typical | Basis |
|---|---|---|
| Tensile strength | 32 ksi (221 MPa) | 20°C; flat products, 0.040-in (1.0 mm) section |
| Yield strength (0.5% extension) | 10 ksi (69 MPa) | Not an Rp0.2 value |
| Elongation | 45% | Gauge length not stated |
CDA typical values for this temper and section only, not specification minima.
Copper Development Association — C10200 alloy record
H02 half hard — flat, CDA typical
| Property | CDA typical | Basis |
|---|---|---|
| Tensile strength | 42 ksi (290 MPa) | 20°C; flat products, 0.040-in (1.0 mm) section |
| Yield strength (0.5% extension) | 36 ksi (248 MPa) | Not an Rp0.2 value |
| Elongation | 14% | Gauge length not stated |
CDA typical values for this temper and section only, not specification minima.
Copper Development Association — C10200 alloy record
H04 hard — flat, CDA typical
| Property | CDA typical | Basis |
|---|---|---|
| Tensile strength | 50 ksi (345 MPa) | 20°C; flat products, 0.040-in (1.0 mm) section |
| Yield strength (0.5% extension) | 45 ksi (310 MPa) | Not an Rp0.2 value |
| Elongation | 6% | Gauge length not stated |
CDA typical values for this temper and section only, not specification minima.
Copper Development Association — C10200 alloy record
Not heat-treatable
These coppers are strengthened only by cold work (H tempers) and softened by annealing (O / OS tempers).
Reducing atmospheres
ETP (C11000) reacts with hydrogen at elevated temperature: hydrogen combines with internal cuprous oxide forming steam and causing embrittlement. OF and OFE resist this oxide-related mechanism.
Oxide test
ASTM B577 is a test method for cuprous oxide in oxygen-free and deoxidised copper; ASTM B170 Grade 1 (C10100) requires ten reverse bends and Grade 2 (C10200) eight after B577 Method D.
No specific annealing temperatures are given here; agree temper with the product specification.
ASTM B577 — official listing
Typical applications
Engineering applications
- Electrical conductors and bus bars
- Hydrogen-brazed and vacuum components
- Electronic components
Subsequent manufacturing
Machining & processing
Brazing and vacuum use
Select OF or OFE for hydrogen brazing, vacuum electronics and reducing atmospheres; ETP is not suitable for these conditions.
Forming
All three cold-form readily; strength rises and conductivity falls slightly with cold work.
Application evidence
Listed applications are source-cited categories, not claims of stock or component approval.
Material certification & testing
Documentation must be agreed for the actual UNS/EN grade, product specification, form, temper and any conductivity or oxygen-content test.
No certificate, conductivity guarantee, approval or grade equivalence is automatic; quotation controls remain disabled.
- EN 10204 3.1 material certificate, where agreed with the supplier
- Certificate of Conformity
- Cast / lot traceability to the producing mill
- Chemical analysis, including oxygen where specified
- Electrical conductivity and mechanical test results for the supplied temper, where ordered
Material enquiry
Request a material quotation