Materials Supply / Controlled-Expansion & Electronic Alloys
Alloy 52 (Fe–52Ni sealing alloy)
Fe–51/52Ni | UNS N14052 | EN 1.3923 / 2.4478
Alloy 52 has the highest nickel of the Fe–Ni sealing alloys listed, used for seals to soft glasses.
No primary producer CTE, physical or mechanical tables were verified; none are borrowed from Alloy 48.
Imagery is illustrative metal product forms, not certified Alloy 52 stock or evidence of Quest stockholding.
Raw & semi-finished materials
Available material forms
Aperam and VDM list bar, strip and wire. Confirm forms, sizes and availability at enquiry.
- Rod and bar
- Cold-rolled strip
- Drawn and flat wire
Material overview
Alloy 52 (Fe–52Ni sealing alloy)
A 51–52% nickel–iron sealing alloy for soft-glass seals; producer numerical property data were not verified.
- Thermal-expansion values are withheld: no primary producer table with stated interval was accessed.
- Aperam (FeNi52) and VDM (Ni 51) nominal chemistries differ — real source differences, not limits.
Designations and specifications
| Designation / standard | Scope and qualification |
|---|---|
| UNS | N14052 (Aperam, VDM) |
| European | EN 1.3923 (Aperam); 2.4478 (Aperam, VDM) |
| Producer names | Aperam IMPHY N52; VDM Alloy 52 / Pernifer 50 |
| ASTM F30 | Fe–Ni sealing alloys — withdrawn |
Specification review
Technical verification requirements
All numerical properties
No primary CTE, physical, mechanical or annealing data verified.
Obtain producer datasheet.
Grade selection
Controlled-expansion alloys — distinct grades, not substitutes
| Alloy | Nominal base (mass %) | UNS (as verified) | Published mean CTE and interval | Primary intended use (per source) |
|---|---|---|---|---|
| Invar 36 | Fe–36Ni | K93601 / K93603 (Carpenter) | 1.30 × 10⁻⁶/K to 93°C; lower reference not stated (Carpenter) | Dimensionally stable structures, tooling, instruments |
| Super Invar | Fe–32Ni–5.5Co | K93500 (Carpenter) | 0.63 × 10⁻⁶/K, −55 to 95°C (Carpenter) | Lower expansion than Invar 36 over a narrow range |
| Kovar | Fe–29Ni–17Co | K94610 (ASTM F15) | 5.85 × 10⁻⁶/K, 25–100°C; 5.13 × 10⁻⁶/K, 25–300°C (Carpenter, annealed) | Seals to hard borosilicate glass and alumina ceramics |
| Alloy 42 | Fe–41/42Ni | K94100 (Carpenter, VDM) | 5.40 × 10⁻⁶/K, 21–343°C (Carpenter); 5.3 × 10⁻⁶/K, 20–300°C (NILO 42) | Glass sealing (e.g. 1075, 0120, 0010 glasses per Carpenter), lead frames |
| Alloy 46 | Fe–46Ni(–0.4Ti, Carpenter) | Not verified | Not verified | Enamelled-resistor terminal bands (Carpenter) |
| Alloy 48 | Fe–48Ni | K94800 (Special Metals, Aperam) | 8.7 × 10⁻⁶/K, 20–300°C (NILO 48) | Soft lead or soda-lime glass seals |
| Alloy 52 | Fe–51/52Ni | N14052 (Aperam, VDM) | Not verified from a primary producer table | Soft-glass seals (Aperam) |
Each value keeps its own producer, interval and conditioning; values from different sources are not directly comparable. Glass-to-metal sealing requires matching the alloy expansion curve to the specific glass or ceramic over the whole sealing-to-service temperature range — Kovar and Alloys 42/46/48/52 are not interchangeable.
Engineering reference
Technical data
| Element | Aperam IMPHY N52 | VDM Alloy 52 |
|---|---|---|
| Nickel | 52 (indicative) | 51 (typical) |
| Iron | Balance | 49 |
Nominal values only; impurity limits not verified.
| Property / condition | Verified value | Required basis |
|---|---|---|
| Tensile, ductility and hardness | Not verified from a primary producer source | Ordered specification, product form, temper and test basis |
No primary producer mechanical data were verified for Alloy 52; distributor transcriptions were not used. Acceptance data must be agreed for the ordered specification and condition.
| Property | Verified value | Basis |
|---|---|---|
| Mean CTE, density, modulus, Curie / inflection temperature | Not verified | No primary producer table accessed; Alloy 48 values not substituted |
Obtain a producer datasheet stating CTE interval and conditioning for the ordered material.
Typical applications
Engineering applications
- Seals to soft glasses (Aperam)
- Controlled-expansion electronic parts
Subsequent manufacturing
Machining & processing
Machining and forming
Machining and cold forming introduce residual stress that changes expansion behaviour and dimensional stability; final stabilising or annealing treatments should follow rough machining, near final size.
Magnetic transformation
The low-expansion range of these Fe–Ni(–Co) alloys ends near their Curie (or inflection) temperature; above it, expansion rises sharply. Do not extrapolate a mean CTE beyond its stated interval.
Not a corrosion-resistant alloy
These alloys are not stainless; protection must be specified for humid or corrosive service.
Application evidence
Listed applications are producer-cited categories, not claims of stock or component approval.
Material certification & testing
Documentation must be agreed for the actual alloy, specification, product form, temper and any expansion-test requirement. Expansion acceptance depends on the specified interval and pre-test conditioning.
No certificate, expansion guarantee, sealing approval or alloy equivalence is automatic. Low-expansion and sealing alloys are not interchangeable; quotation controls remain disabled.
- EN 10204 3.1 material certificate, where agreed with the supplier
- Certificate of Conformity
- Heat / batch traceability to the producing mill
- Chemical analysis to the ordered specification
- Thermal-expansion test report over the specified interval and conditioning, only where ordered
Material enquiry
Request a material quotation
Alloy 52 (Fe–52Ni sealing alloy) supplied to your material form, dimensions and specification.