Alloy 48 (Fe–48Ni sealing alloy)
Fe–48Ni | UNS K94800 | EN 1.3922
Alloy 48 has a higher, flatter expansion than Alloy 42 up to an inflection near 460°C (Special Metals), suiting soft glasses.
It is not interchangeable with Kovar or Alloys 42, 46 or 52 for sealing.
Imagery is illustrative metal product forms, not certified Alloy 48 stock or evidence of Quest stockholding.
Raw & semi-finished materials
Available material forms
Aperam lists bar and cold-rolled strip for IMPHY N48. Confirm forms, sizes and availability at enquiry.
- Bar
- Cold-rolled strip
Material overview
Alloy 48 (Fe–48Ni sealing alloy)
A 48% nickel–iron alloy with higher expansion than Alloy 42, matched to soft lead and soda-lime glasses.
- Mean CTE is from Special Metals NILO 48, from 20°C to each stated temperature; condition not stated.
- Aperam lists both sealing (F30) and magnetic (A753) identifiers; these are not a universal equivalence.
Designations and specifications
| Designation / standard | Scope and qualification |
|---|---|
| UNS | K94800 (Special Metals, Aperam); Aperam also lists K94840 |
| European | EN 1.3922 (Aperam) |
| Producer names | Special Metals NILO 48; Aperam IMPHY N48 |
| ASTM F30 | Fe–Ni sealing alloys — withdrawn |
| ASTM A753 | Nickel–iron soft magnetic alloys (listed by Aperam) |
Specification review
Technical verification requirements
Mechanical / chemistry
Only hardness and nominal Ni verified.
Obtain full producer datasheet.
Grade selection
Controlled-expansion alloys — distinct grades, not substitutes
| Alloy | Nominal base (mass %) | UNS (as verified) | Published mean CTE and interval | Primary intended use (per source) |
|---|---|---|---|---|
| Invar 36 | Fe–36Ni | K93601 / K93603 (Carpenter) | 1.30 × 10⁻⁶/K to 93°C; lower reference not stated (Carpenter) | Dimensionally stable structures, tooling, instruments |
| Super Invar | Fe–32Ni–5.5Co | K93500 (Carpenter) | 0.63 × 10⁻⁶/K, −55 to 95°C (Carpenter) | Lower expansion than Invar 36 over a narrow range |
| Kovar | Fe–29Ni–17Co | K94610 (ASTM F15) | 5.85 × 10⁻⁶/K, 25–100°C; 5.13 × 10⁻⁶/K, 25–300°C (Carpenter, annealed) | Seals to hard borosilicate glass and alumina ceramics |
| Alloy 42 | Fe–41/42Ni | K94100 (Carpenter, VDM) | 5.40 × 10⁻⁶/K, 21–343°C (Carpenter); 5.3 × 10⁻⁶/K, 20–300°C (NILO 42) | Glass sealing (e.g. 1075, 0120, 0010 glasses per Carpenter), lead frames |
| Alloy 46 | Fe–46Ni(–0.4Ti, Carpenter) | Not verified | Not verified | Enamelled-resistor terminal bands (Carpenter) |
| Alloy 48 | Fe–48Ni | K94800 (Special Metals, Aperam) | 8.7 × 10⁻⁶/K, 20–300°C (NILO 48) | Soft lead or soda-lime glass seals |
| Alloy 52 | Fe–51/52Ni | N14052 (Aperam, VDM) | Not verified from a primary producer table | Soft-glass seals (Aperam) |
Each value keeps its own producer, interval and conditioning; values from different sources are not directly comparable. Glass-to-metal sealing requires matching the alloy expansion curve to the specific glass or ceramic over the whole sealing-to-service temperature range — Kovar and Alloys 42/46/48/52 are not interchangeable.
Engineering reference
Technical data
| Element | Mass % |
|---|---|
| Nickel | 48 (nominal) |
| Iron | 52 / balance |
Special Metals and Aperam give nominal FeNi48 only; impurity limits not verified.
| Property / interval | Producer value | Basis |
|---|---|---|
| Density | 8.20 g/cm³ | — |
| Elastic modulus | 160 GPa | Temperature not stated |
| Thermal conductivity | 16.7 W/(m·K) | 20°C |
| Electrical resistivity | 47 µΩ·cm | 20°C |
| Inflection temperature | 460°C | Not stated as Curie temperature |
| Mean CTE 20–100°C | 8.5 × 10⁻⁶/K | Condition not stated |
| Mean CTE 20–200°C | 8.6 × 10⁻⁶/K | Condition not stated |
| Mean CTE 20–300°C | 8.7 × 10⁻⁶/K | Condition not stated |
| Mean CTE 20–400°C | 8.8 × 10⁻⁶/K | Condition not stated |
Mean coefficients, not instantaneous.
Annealed — NILO 48 hardness only
| Property | Producer value | Basis |
|---|---|---|
| Hardness | ≤ 80 HRB | Annealed |
| Tensile strength, yield, elongation | Not verified | Not extracted from a primary table |
Only annealed hardness was verified.
Annealing (Special Metals)
850–1000°C in protective atmosphere for maximum dimensional stability.
No quantified effect on expansion published.
Typical applications
Engineering applications
- Seals to soft lead and soda-lime glasses
- Controlled-expansion electronic parts
Subsequent manufacturing
Machining & processing
Machining and forming
Machining and cold forming introduce residual stress that changes expansion behaviour and dimensional stability; final stabilising or annealing treatments should follow rough machining, near final size.
Magnetic transformation
The low-expansion range of these Fe–Ni(–Co) alloys ends near their Curie (or inflection) temperature; above it, expansion rises sharply. Do not extrapolate a mean CTE beyond its stated interval.
Not a corrosion-resistant alloy
These alloys are not stainless; protection must be specified for humid or corrosive service.
Application evidence
Listed applications are producer-cited categories, not claims of stock or component approval.
Material certification & testing
Documentation must be agreed for the actual alloy, specification, product form, temper and any expansion-test requirement. Expansion acceptance depends on the specified interval and pre-test conditioning.
No certificate, expansion guarantee, sealing approval or alloy equivalence is automatic. Low-expansion and sealing alloys are not interchangeable; quotation controls remain disabled.
- EN 10204 3.1 material certificate, where agreed with the supplier
- Certificate of Conformity
- Heat / batch traceability to the producing mill
- Chemical analysis to the ordered specification
- Thermal-expansion test report over the specified interval and conditioning, only where ordered
Material enquiry
Request a material quotation
Alloy 48 (Fe–48Ni sealing alloy) supplied to your material form, dimensions and specification.